Cement Base Plastering Render Repair Mortar with high strength
Product features:
1. Extremely low water demand, have good early strength.
2. Excellent bonding power, reduce the old and new mortar's stripping.
3. High density, good waterproof performance. Reduce permeability of chloride and carbon dioxide, protect building's main structure effectively.
4. Low shrinkage, reduce cracking.
5. Easy construction so that improve the efficiency.
6. Non-toxic and tasteless, it does not contain solvent, inflammable.
Scope of application:
It’s suitable to repair concrete exfoliation caused by reinforcement corrosion; repair the structural defects or concrete components part; fill in the gap between the decorative window.
Construction technology:
Base treatment: Before construction, cut into the maintenance scope about 10 mm with cutting machine, chiseling all loose concrete away, remove rust iron thoroughly, and remove dust on the surface of the concrete, And then coated with repair mortar interface agent on the steel surface. If the base plane is dry completely before plastering repair mortar, must be clean with water thoroughly and plaster again, and then can plaster the repair mortar.
Stirring: mix mortar with quantitative water (add water gradually), stirring with the right type of blender mixing about 5 min, until evenly without block.
Construction: Put and overwhelm the repair mortar with a spatula or with artificial construction directly on the base plane of the coating interface. In general, the thickness of single-layer is 30 mm, if the coating is so thick that it drops down, you must wipe out the affected parts. And plastering a thinner mortar on it again. Thicker parts maintenance need to daub in multilayer daub manner. Please scrape the next coating after the first coating is completely dry.
Maintenance: Exposed surface need to maintenance after construction, it can use the suitable curing agent, watering continuous and other maintenance ways.
Attention:
1. Should clean and wet the base plane before construction.
2. The stirred slurry should be finished within 4 hours.
3. Avoid construction below 5 , 40 above environment.
4. The layer is completed, should be natural maintenance more than 3 days, can do the next working procedure construction.
5. Don’t use the dried paste by re-adding water.
Technical Parameter:
Execute standard JG/T 336-2011
Testing Items Testing description Standard requirement and result
Setting time Initial/min ≥45
Final/h ≤12
Compressive strength / Mpa 7d ≥10.0
28d ≥15.0
Flexural strength/ Mpa 7d ≥4.0
28d ≥6.0
Tensile adhesive strength/Mpa No treatment 28d ≥1.0
In water 28d ≥0.8
25times freeze-thaw cycle 28d ≥0.8
Shrinkage ratio % 28d ≤0.10
Storage
Avoid direct sunlight and storage on plate from the ground.
12 months stored in the cold and dry place.
Spec.
25kg/bag